The phenomenon in austenitic stainless steels that causes a change to occur in the grain boundaries when heated in the general range of 850 to 1,475°F. This change destroys the passivity in these locations.
Sensitization:
In austenitic stainless steels, the precipitation of chromium carbides, usually at grain boundaries, on exposure to temperatures of about 540 to 845°C (about 1000 to 1550 °F), leaving the grain boundaries depleted of chromium and therefore susceptible to preferential attack by a corroding medium. Welding is the most common cause of sensitization. Weld decay (sensitization) caused by carbide precipitation in the weld heat-affected zone leads to intergranular corrosion.
A
|
B
|
C
|
D
|
E-G
|
H-I
|
J-L
|
M-N
|
O-P
|
Q-R
|
S
|
T
|
U-W
|
X-Z
|
#
Submit Term
Comments/questions, please contact AIST Member Services at (724) 814-3000, ext. 1 or
memberservices@aist.org
Association for Iron & Steel Technology
186 Thorn Hill Road • Warrendale, PA 15086-7528 USA
(724) 814-3000 • Fax: (724) 814-3001
AIST Privacy Statement
•
Trademarks and Ownership